Quick answer: Blister forming webs run from plain PVC through PVDC-coated PVC and PCTFE laminates to cold-form aluminium, and moisture barrier rises along that line. Mono-material PET and PP films, which suit recycling streams, currently cover the low-to-medium barrier end. Which rung a product needs is settled through stability data and your regulatory and quality teams, not by the packaging engineer alone.
This piece rests mainly on converter, machine-builder and instrument-maker pages (JinLu Packing, Jornen, Tiptop, Pharmaworks, TekniPlex, Lighthouse, Sepha) plus a consultancy white paper; independent test data is noted where it exists. It is education only: nothing here says a film is compliant or right for any drug or dose form.
Why blisters are in the news this week
As of 11 November 2026, Sustainable Packaging News reports that CHP Australia members have backed a mail-back satchel for empty medicine blister packs. Retail Pharmacy says it launched in National Recycling Week (9 to 15 November) and is subsidised, at $9.95 including return postage (Australian dollars, as the scheme is Australian).
The recycler is Pharmacycle, which says blister packs cannot be recycled through kerbside recycling because they combine plastic and aluminium. Its locator page describes mechanical separation of foil from plastic by shredding, grinding, air-density separation and electrostatic separation. That is a clean-up of the end-of-life problem, and the structures below are where the problem starts.
The PVC family: plain, PVDC-coated and PCTFE-laminated
Rigid, unplasticised PVC is the baseline forming web. Most pharmaceutical PVC sheet is 250 µm thick, and Jornen gives a typical WVTR of around 3.0 g/m2/day at 38 °C and 90% RH, with OTR around 20 mL/m2/day. The same page points to USP <661> among the references a PVC formulation has to meet.
PVDC is coated onto the PVC to cut permeation. JinLu Packing lists 250 µm PVC with 40 to 120 g/m2 PVDC at roughly 0.65 to 0.25 g/m2/day WVTR, and an example of 80 g/m2 at about 0.30 g/m2/day. These are typical supplier figures at 38 °C and 90% RH, not specifications.

Source: JinLu Packing technical page on PVC vs PVDC (typical supplier figures, not specifications)
Our calculation: 3.0 ÷ 0.65 = 4.6, and 3.0 ÷ 0.25 = 12. So the coating cuts WVTR by about 4.6 to 12 times across that coat-weight range, against the 5 to 10 times the same page quotes.
PCTFE (the film sold as Aclar) is laminated to PVC for higher barrier. One published description gives 250 µm PVC laminated to 15 to 150 µm PCTFE and typical WVTR of 0.06 to 0.40 g/m2/day. Conditions aren’t always stated for these laminate figures, so check them before comparing with the PVC baseline. The PVC layer is retained because foil with a heat-seal coating bonds to PVC but not to PCTFE.
Cyclic olefin copolymer (COC) is the other add-on. It can be laminated to PVC, or sandwiched between two PP layers, which REAP Consulting dates to the late 1990s for medium-to-high moisture barrier.
Free tool: the unit converter turns coat weight in g/m2 and film thickness in µm into one another when you’re comparing supplier sheets.
Cold-form aluminium: the hermetic option with geometry limits
Cold-form (“alu-alu”) web is a laminate of oriented polyamide (OPA), aluminium foil and PVC, formed by deep-drawing at room temperature. A converter page from aluminumblister.com gives a typical build of OPA 25 to 30 µm, aluminium 45 to 60 µm and PVC 60 µm, 140 to 160 µm in total. A second maker, Tiptop, lists weights of 245 to 300 g/m2 across five aluminium gauges. Another supplier page puts total thickness at 120 to 200 µm.
The layers split the work. The OPA carries most of the multi-axial forming, the aluminium gives the barrier, and the PVC is the sealing side. Makers describe the barrier to moisture, oxygen and light as near complete, but they quote no WVTR figure, so ask for data.
Cavity depth is the practical constraint. A machine builder’s guide (Hij Packing Machine) suggests that cavities deeper than 12 mm need thermoforming, while 9 mm or less is feasible for cold-forming. Treat that as a rule of thumb from one vendor.
Mono-material films: PET, PP and the barrier gap
PVC-free structures are being assessed for recycling streams. Healthcare Packaging reports on a Pharmaceutical Manufacturing Forum workstream that expects sustainable blisters to be 100% polymeric, with possible difficulty matching existing barrier. It adds that regulators could be engaged on simulation models to reduce stability testing.
The barrier gap is quantified by REAP Consulting: an all-PET blister has an MVTR at least 4 times higher than a PVC/Al blister. The same article says that above 120 g/m2 PVDC or 51 µm PCTFE, there are no recyclable monopolymer options in sight; the paper is from 2025 and the market may have moved. TekniPlex has launched a transparent mid-barrier polyolefin/PP blister it certifies as recyclable where a #5 PP stream exists (company claim, per Pharmaceutical Technology).
Machines matter too. Pharmaworks says mono films have a tighter heat tolerance and tend to stretch after thermoforming, and sealing is harder without an adhesive laminate. Expect a narrower process window, and plan trials accordingly.
Side-by-side comparison
| Structure | Typical WVTR (g/m2 day, 38 °C, 90% RH) | Forming | Recycling note |
|---|---|---|---|
| PVC, 250 µm | about 3.0 | Thermoform | PVC plus foil lid; multi-material |
| PVC with PVDC coat (40 to 120 g/m2) | 0.65 to 0.25 | Thermoform | As above, plus PVDC |
| PVC/PCTFE (15 to 150 µm PCTFE) | 0.06 to 0.40 (conditions vary) | Thermoform | As above, plus PCTFE |
| Cold-form OPA/Al/PVC | No figure quoted; described as near complete | Cold-form, depth limits | Aluminium-polymer laminate |
| Mono-PET | At least 4 times PVC/Al | Thermoform | Aimed at PET streams |
| PP/COC/PP | Medium barrier | Thermoform | Aimed at PP stream |
Use the numbers to rank options, not to predict shelf life. Film-level WVTR differs from finished-pack moisture ingress, which also depends on cavity shape, seal width and lidding foil.
Seal integrity testing for blisters
Container closure integrity (CCI) for blisters is about the seal. The reference chapter is USP <1207>, which, Lighthouse Instruments notes, does not set a universal leak-rate limit. A Eurofins summary says the 2016 guidance prefers deterministic methods over probabilistic ones.
Dye ingress is the probabilistic example. Sepha calls it cheap and easy but subjective, time-consuming and destructive. Vacuum decay (ASTM F2338) is the deterministic counterpart: it monitors vacuum level in a test chamber for decay that indicates a leak.
Blisters complicate this. A patent filing on blister leak detection argues that small multi-cavity packs hold too little air for simple vacuum decay and that such tests don’t say which cavity is leaking. JinLu Packing’s blister seal testing page notes that ASTM F3169 addresses vacuum deflection for blisters. Which method is validated for your pack is a quality-team decision.
Questions for suppliers, regulatory and quality teams
Suppliers:
- Which test method and conditions sit behind each WVTR and OTR figure, and was it measured on film or on formed, sealed packs?
- What is the coat weight or layer gauge, and what is the tolerance?
- What is the forming window (temperature, cavity depth, draw ratio) and the sealing window on my line?
- Which recycling claim is made, under which scheme, and for which collection streams?
Regulatory and quality:
- Which pharmacopoeial chapters and food-contact or extractables requirements apply to this web and lidding, in each target market?
- Does a change of web need new stability data, and could simulation models reduce it?
- Which CCI method is validated for this blister format, and what leak size does it detect?
What this means for you
Start from the product’s moisture and light sensitivity as set out by your formulation and stability teams, then read the table from the top. If the data points to the high-barrier end, mono-material films may not be an option yet, and the end-of-life route is a collection scheme like Pharmacycle’s rather than kerbside.
If the data allows low or medium barrier, ask suppliers for PET, PP and PP/COC/PP quotes alongside your current web, and ask for ranges, not single points. Plan machine trials, since mono films have narrower windows.
Free tool: the laminate estimator gives an indicative layer-stack weight and barrier when you want a first comparison before supplier data arrives.
Recycled-content and recyclability rules for packaging in the EU are changing; for the plain-language detail, see ppwreu.org and check the current text before you rely on any claim.
Sources
- Sustainable Packaging News: CHP Australia members take voluntary collective action to make blister pack recycling more accessible
- Retail Pharmacy: CHP Australia members take voluntary collective action to make blister pack recycling more accessible
- Pharmacycle: Store drop-off locator and FAQ
- Pharmacycle: ABC War on Waste
- Jornen: What is difference between PVC and PVDC
- JinLu Packing: PVC vs PVDC, which is right for your pharmaceutical packaging
- USPTO: Critical temperature indicator (patent 8562208, PCTFE and PVC background)
- USPTO: Disposable beverage container (patent 8973775, blister film background)
- Pharma Treasures: Benefits of PVDC over PVC as a primary packaging material
- aluminumblister.com: Alu Alu Cold Forming Foil
- Tiptop: Cold Formable Blister Alu-Alu
- Luoyang Dirante: Cold Forming Foil and PTP Blister Foil
- Hij Packing Machine: PVC vs PVDC vs ALU-ALU foil blister material guide
- Healthcare Packaging: The many facets of sustainable and recyclable blister packaging
- REAP Consulting: The future of sustainable pharma blister packaging
- Pharmaceutical Technology: New blister packaging options
- Pharmaworks: Blister machine compatibility with mono-material films
- Lighthouse Instruments: USP 1207 container closure integrity testing
- Eurofins BPT: Container closure integrity testing
- Sepha: USP 1207, opening the CCIT toolbox
- USPTO: Method and apparatus for detecting leaks in blister packs (patent 7665346)
- JinLu Packing: Blister seal integrity testing
This article is general education about packaging materials, formats and test methods. It is not regulatory, quality or medical advice. For a real product, confirm material choice, testing and compliance with your regulatory and quality teams and the applicable pharmacopoeia and authority.