Quick answer: This glossary is for packaging engineers, R&D and procurement staff, quality teams and students who need to read a sealant data sheet or a seal test report without a translator. Read it once in order (process, curve, strength tests, leak tests), then use the headings and the table as a lookup. Fifteen terms follow.
This piece rests mainly on ASTM catalogue pages, explainers from test-equipment and test-service firms (Instron, LSO, Industrial Physics and Ametek Mocon all sell testing equipment or services), two academic papers and test descriptions in patents. No sealant supplier data sheets are used.
The sealing process: three settings
1. Heat seal and sealant layer
A heat seal is a melt fusion process: two thermoplastic surfaces are heated until they flow together, then cooled in contact. The sealant layer is the innermost film layer that does the fusing. One handbook chapter describes the ideal hot-bar structure as a temperature-resistant outer layer over an inner layer with a low seal initiation temperature.
Where it shows up: every pouch, lidding and tub spec. The same handbook’s worked example uses OPET 12 µm over a 51 µm sealant. Free tool: the laminate estimator shows how a layer stack adds up in weight.
2. Dwell time
Dwell time is the time the sealing bars are in actual contact with the film. It follows from line speed and the share of the machine cycle spent sealing. In the handbook’s example, 60 packs per minute with half the cycle sealing gives 0.5 s.
Unit: seconds or milliseconds. Where it shows up: every speed-up request, because a shorter dwell time needs a higher seal initiation temperature. A machine patent puts transverse-seal dwell at roughly 0.1 to 1 second, depending on machine speed.
3. Seal pressure
Seal pressure is the clamping force of the jaws spread over the seal area. Many lab test descriptions use 0.275 N/mm2 (40 psi). Its influence is disputed by material: a BioResources paper reviewing earlier work says temperature and dwell time had a major influence on seal strength, and pressure very little. A Packaging Technology and Science study of coffee capsule materials, though, needed at least 207 kPa for enough film contact.
Where it shows up: jaw set-up sheets and the “conditions” line of any seal test report.
Reading a heat seal curve
4. Heat seal curve
A heat seal curve plots seal strength against seal bar temperature. At low temperature there is no seal; strength then rises rapidly at the initiation point, before settling on a plateau. Unit: N per 15 or 25 mm of seal width against °C. Where it shows up: sealant supplier literature and film qualification reports.
5. Seal initiation temperature (SIT or HSIT)
SIT is the minimum temperature at which seal strength is obtained. “Obtained” is defined by whoever writes the report, which is the catch. A low SIT is wanted for high-speed packing, where sealing times are short.
Patent test descriptions show four different thresholds: 200 g per 25.4 mm, 1 lb per inch, 5 N on a 25 mm strip, and 4.4 N per 12.7 mm. These are examples from patents, not standard definitions.
Our calculation (all converted to N per 25.4 mm): 0.2 kg × 9.81 = 1.96 N; 1 lbf = 4.45 N; 5 N × 25.4 / 25 = 5.08 N; 4.4 N × 2 = 8.8 N. The highest threshold is 8.8 / 1.96 = 4.5 times the lowest. Two “SIT” figures only compare if the threshold, dwell, pressure and test method match.

Source: Thresholds from USPTO patents 11708483, 8568894, 12576621 and 10189922; unit conversion is our own calculation
6. Sealing window
The sealing window is the temperature range that gives good seals. The SIT sets its lower end; film distortion and other limits set the upper end. A hot tack description adds the burn-through temperature as an upper limit. The window depends on the film structure and on the sealing conditions, so it moves when the machine does.
Where it shows up: choosing jaw temperature with room for drift, and comparing two sealants for a given line.
7. Hot tack
Hot tack is the force needed to separate a seal while the sealant is still hot and not fully solidified. It matters where a seal is loaded before it cools, such as a bag seal under falling product. The method is ASTM F1921, which gives guidance but does not fix the equipment or conditions.
Unit: N/25 mm. One patent test uses 0.5 s seal time, 0.275 N/mm2 and a 200 mm/s pull. Hot tack initiation is defined as 1 N/25 mm in one source and 2 N in another. A handbook chapter says the breadth of the hot tack range is perhaps more important than the peak value.
Testing the seal after it cools
8. Seal strength
Seal strength is the force to pull a strip apart across the seal. ASTM F88 measures it at ambient temperature, and reports can give average force per unit width over the peel, or the maximum. Unit: N/15 mm or N/25 mm (lb/in in older US sheets).
Conditions matter: specimen width, a lab grip speed of 200 to 300 mm/min in one lab’s procedure, 500 mm/min in a patent, and conditioning at 23 °C.
9. Peel, peelable seal and permanent seal
Peel means the two sealing layers separating at the sealing interface. A peelable seal is designed to do that on opening. If the film tears or snaps before the seal peels, no peel number is obtained and the seal counts as permanent.
ASTM F88 has three holding techniques: A, unsupported; B, hand-supported at 90°; and C, a supported 180° fold. The same seal can give different values depending on which you use, and LSO says free-tail usually gives the lowest value.
Where it shows up: lidding films and capsules. One capsule patent describes a preferred peelable seal of about 2 to 12 N for a 25 mm strip.
10. Failure mode
Failure mode records how the seal gave way, not just the force. Test descriptions report maximum force, average peel force and failure mode. A patent separates peeling at the interface from breaking, where the seal fractures. Film tear before peel means the number reflects the film, not the seal.
11. Seal contamination and caulkability
Contamination is product in the seal area, such as powder, fat or liquid. Caulkability describes a sealant’s ability to encapsulate contamination or flow into voids in the seal area so the pack doesn’t leak. The coffee capsule paper above tested coffee particles of 0.70 to 0.85 mm in the seal.
Where it shows up: powder, snack and coffee lines, where the seal closes through product.
Pressure and leak terms
12. Burst test
A burst test inflates a sealed pack until it fails. ASTM F2054 finds the minimum burst strength of a perimeter seal inside restraining plates; ASTM F1140 is the unrestrained version, which tests overall pressure resistance including the film. Plates matter because without them, stress isn’t spread evenly across the seal. F2054 also notes it may not correlate with F88 or F1140 seal strength.
Unit: pressure at failure (psi in the patent examples). Where it shows up: whole-pack seal checks, including transit and altitude concerns.
13. Pressure decay leak test
Pressure decay inflates the pack, closes the valves and watches the pressure. Ametek Mocon says the test pressure is typically 10 to 30 percent of burst pressure, and a pressure loss indicates a leak. ASTM F2095 detects leaks of 1 × 10^-4 sccs or greater, with method A unrestrained and method B using restraining plates. It covers nonporous pouches and foil-sealed trays and is destructive, since it needs entry into the pack.
14. Channel leak
A channel leak is a continuous path through the seal width, often from a wrinkle, a fold or trapped product. Peel tests measure force, not whether a path exists. A dye test shows one when dye reaches the other side of the seal.
15. Dye penetration test
ASTM F1929 applies dye to the seal edge and looks for leakage. It detects a leak equal to or greater than a channel formed by a 50 µm wire, on seals between a transparent material and a porous sheet. The result is pass or fail, not a leak size; it is destructive; and dye goes on by injection, edge dip or eyedropper. ASTM F3039 is the non-porous counterpart.
This is a description of a method only. It is used within sterile barrier integrity strategies under ISO 11607, but which test fits a pack is decided with your regulatory and quality teams and the applicable standard or pharmacopoeia.
Quick reference table
| Test | Standard | What it reports | Typical unit |
|---|---|---|---|
| Seal strength (peel) | ASTM F88 | Force to peel a strip across the seal | N/15 mm or N/25 mm |
| Hot tack | ASTM F1921 | Strength of the still-hot seal | N/25 mm |
| Burst | ASTM F2054, F1140 | Pressure at which seal or pack fails | Pressure |
| Pressure decay | ASTM F2095 | Pressure loss showing a leak | Pressure drop or sccs |
| Dye penetration | ASTM F1929 | Visible dye path through a seal | Pass or fail |
Standards are revised, so check the current edition. The sources above cite F88/F88M-21, F2054-13(2020), F2095-07(2021) and F1929-23.
What this means for you
When a supplier quotes a seal initiation temperature, ask four things: the strength threshold, the dwell time, the pressure and the test method. Better, ask for the full heat seal curve and hot tack curve, because a single number hides the window.
Calculate your own dwell time from line speed with the sum in term 2, and ask for data at that dwell, not at a convenient lab setting. When you receive F88 results, ask for the technique (A, B or C), strip width, grip speed and failure mode alongside the force.
For leaks, ask which test would actually find a channel, since peel force won’t. Agree whether you need a pass/fail check, a leak rate or a burst pressure, and say whether packs are restrained. Free tool: the printable checklists are a starting point for your own supplier question list.
For sterile barrier or other pharma-related packs, take method choice and acceptance limits to your regulatory and quality teams.
Sources
- Instron: ASTM F88 Seal Strength of Flexible Barrier Materials
- LSO: ASTM F88 Peel Testing for Medical Packaging
- LSO: ASTM-F88 for Seal Strength Testing
- Westpak: Seal Strength Test (Seal Peel Testing)
- ASTM: F2054 Burst Testing of Flexible Package Seals Using Internal Air Pressurization Within Restraining Plates
- iTeh Standards: ASTM F2054/F2054M-13(2020)
- Industrial Physics: Burst Testing, Glossary and Key Facts
- ASTM: F2095-07(2021) Pressure Decay Leak Test for Flexible Packages
- ASTM: F2095-01 Pressure Decay Leak Test for Nonporous Flexible Packages
- Ametek Mocon: ASTM F2095 leak test via pressure decay
- ASTM: F1929 Detecting Seal Leaks in Porous Medical Packaging by Dye Penetration
- ANSI Blog: ASTM F1929-23 Seal Leaks in Porous Medical Packaging
- LSO: ASTM F1929 Dye Penetration Testing
- LSO: Dye Penetration Testing for Medical Device Packaging
- iTeh Standards: ASTM F1929-23 Seal Leak Detection in Porous Medical Packaging
- Flexpak: Dye Penetration Test Packaging, When You Need It
- ScienceDirect Topics: Seal Initiation Temperature
- ScienceDirect Topics: Hot Tack
- Infinita Lab: ASTM F1921 Hot Seal Strength (Hot Tack) Testing Explained
- Packaging Technology and Science: Effect of heat-sealing parameters on the thermal profile and seal strength of multilayer films and non-woven
- BioResources: Heat sealing evaluation and runnability issues of flexible paper materials in a VFFS machine
- USPTO: US 10189922, Very low density polyethylene produced with single site catalyst
- USPTO: US 8568894, Films and articles with good taste and/or odor performance
- USPTO: US 12576621, Adhesiveless thermally laminated barrier heat sealing films
- USPTO: US 11708483, Heat sealable films
- USPTO: US 12570841, Polyethylene compositions
- USPTO: US 8835567, Sealant composition, method of producing the same
- USPTO: US 10603884, Multi-layer film
- USPTO: US 12172826, Beverage preparation capsules
- USPTO: US 10053565, Ethylene interpolymer films
- USPTO: US 9028935, Packaging machine and packages made therewith
Values are typical figures from the cited sources. Real performance depends on the grade, the test method and the conditions. Check the supplier's data sheet and test your own structure.
Header image: illustration, AI-generated.