Quick answer: For an oxygen-sensitive food in a recyclable PE pouch, a thin EVOH core kept to 5 percent of pack weight or less is the route RecyClass has tested, and AlOx without extra coatings is the transparent alternative. Metallised PE or PP films post low OTR and WVTR figures on supplier sheets, but they are opaque and RecyClass treats them differently by PE stream. The web (MDO-PE, BOPE or BOPP) is a separate decision from the barrier layer, and the data sheet of your actual grade settles both.
This piece rests mainly on supplier statements from Dow, NOVA Chemicals, Inteplast, BOBST, Aropack, CloudFilm and Jijid, several of whom sell the films discussed, so their figures are marketing-grade until you see the full sheet. The recyclability positions come from RecyClass, an independent industry initiative.
The web and the barrier are two choices
A mono-material pouch usually has an oriented outer web for stiffness and print, and a sealant. The outer web is where MDO-PE, BOPE and BOPP compete; the barrier is a layer or coating added on top.
NOVA Chemicals says its MDO-HDPE (based on SURPASS HPs153-A) can replace BOPP and BOPET in all-PE laminates, and that MDO-LLDPE gives toughness comparable to BOPA. MDO stretches a film in one direction; stretching a cast sheet in both directions gives a biaxially oriented film. A published US patent on MDO/BOPE laminates describes why the two get paired: MDO film is stiff in the machine direction but weak across it, while BOPE is the reverse, so the laminate evens out.
On BOPE, Dow’s brochure for its INNATE TF-BOPE resin (1.7 g/10 min melt index, 0.926 g/cm3 density) claims twice the stiffness and about one fifth of the haze and 1.5 times the gloss of 90 µm blown PE, when comparing a 40 µm BOPE film. A Dow conference deck from 2019 reports that a 40 µm BOPE film has stiffness similar to a 90 µm blown film. Both are Dow claims on Dow resin.
BOPP is the benchmark on stiffness and optics. A ScienceDirect overview lists 20 µm BOPP at 2,000 N/mm2 MD modulus, with OTR of 1,600 cc/m2 day and WVTR of 6.0 g/m2 day (the extract doesn’t give test conditions). Supplier sheets such as Aakash’s list haze of 1.5 to 2.0 percent maximum by ASTM D1003. For comparison, Inteplast’s clear 25 µm BOPE grade D1K lists 9 percent haze and an MD modulus of 202,000 psi, which is roughly 1,390 MPa (our conversion at 0.006895 MPa per psi). Different suppliers, different grades; treat it as a scale check only.
The catch for all three: none is a useful oxygen barrier on its own. That is where the next layer comes in.
Barrier routes compared
The table collects figures as the sources state them. They are typical values from supplier or converter pages, not specifications, and test conditions differ, so don’t rank rows by a single number.
| Barrier route | OTR (cm3/(m2 day)) | WVTR (g/(m2 day)) | Conditions as stated | Main weak point |
|---|---|---|---|---|
| EVOH core in PE (PE/EVOH/PE) | Below 0.5 for a 3 to 5 µm EVOH layer; below 1 in mono-PE structures | Not given | Aropack, 25 µm basis; dry state | Humidity |
| AlOx-coated film | 0.5 to 2 | 0.5 to 2 | Jijid, typical range; conditions not stated | Cracks on folding or stretch |
| MDO-PE with oneBARRIER and AlOx GEN II | Below 1 | Below 1 (about 2 for AlOx GEN II with primer alone) | BOBST, with Dow, Zermatt and Sun Chemical | Multi-supplier stack |
| Metallised BOPE, 25 µm (Inteplast M1K) | 3.1 | 0.23 | Converted from cc and g per 100 in2; conditions not in the extract | Opaque |
| Metallised BOPP | 1.0 or below | 0.5 or below | CloudFilm target: 23 °C; 38 °C and 90% RH | Opaque; stream status |
| Metallised OPP, 25 µm | 50 to 100 | 0.3 to 0.8 | Aropack typical range | Weak oxygen barrier |
Sources: Aropack, Jijid, BOBST, Inteplast, CloudFilm.
The two metallised BOPP and OPP rows disagree by a factor of 50 or more on OTR. Different base films, thicknesses, metal densities and test methods could explain it, and the sources don’t say. Ask for the test report, not the headline number.

Source: Inteplast BOPE data sheet (converted from cc per 100 in2 per day), ScienceDirect Topics, Aropack, Jijid; test conditions differ by source
The chart shows the upper end of each quoted figure, so the oxygen-barrier gap between unbarriered and barrier films is visible: roughly 3,410 and 1,600 for the clear BOPE and BOPP, against 100 or less for every barrier route. Conditions vary by source, as the table notes.
Our calculation: Inteplast lists the clear D1K and metallised M1K grades at the same 25 µm and the same modulus, so they share a base. Converting 220 cc per 100 in2 per day (100 in2 = 0.0645 m2) gives 220 ÷ 0.0645 = about 3,410 cm3/(m2 day), against 0.20 ÷ 0.0645 = about 3.1 for M1K, a drop of roughly 1,100 times. WVTR falls from 0.48 to 0.015 g per 100 in2 per day, about 32 times (7.4 to 0.23 g/(m2 day)). The conditions weren’t in the extract, so check the full sheet.
EVOH: the strong dry barrier with a humidity problem
EVOH is coextruded as a thin core, always protected by PE or PP on both sides. Jijid describes it as an outstanding dry oxygen barrier that is coextrudable and flex-resistant, and says it must be encapsulated for moisture shielding.
The moisture sensitivity is large. Aropack states that at 80 percent RH the OTR of EVOH can rise 10 to 50 times against its dry-state value. A wet-filled or humid-chain product therefore needs the barrier figure at the right humidity, not the dry catalogue number.
For PP, Polifilm offers EVOH barrier films with barrier layers of 2 to 25 µm, and says a thin EVOH layer lets the structure stay mainly PP.
AlOx and SiOx: transparent, but they crack
Ceramic coatings are applied in nanometre-scale layers on a base film. Jijid notes AlOx coatings tend to crack under folding and heavy stretching, which degrades the barrier. A Jindal-related patent describes a test that emulates the damage a film takes passing through the forming collar of a VFFS machine, which is the same concern from the machine side: the coated film’s barrier after forming is the number that matters.
BOBST’s mono-PE route pairs MDO-PE with its AlOx GEN II process and a primer, with no topcoat. The company reports that primers A and B with AlOx GEN II reached WVTR of about 2 g/(m2 d) and OTR below 1 cm3/(m2 d), and that the full oneBARRIER stack reaches below 1 on both. That page is an older announcement, so confirm what is commercially available today.
On PP, Jindal Films’ mono-material brochure lists Alox-Lyte and Bicor coated BOPP films as replacements for SiOx or AlOx vacuum-coated PET. The brochure is an older document and its barrier table is hard to read in extract, so quote no numbers from it without the current sheet.
What RecyClass says about each route
The EU packaging regulation (PPWR) and national EPR schemes lean on design-for-recycling criteria of this kind. Check the current text at ppwreu.org; what follows is the voluntary RecyClass position as of 4 November 2026.
On EVOH, RecyClass lab work found up to 5 percent of film weight has a minor effect on recycled PE, while above that the extrusion process was immediately affected. Above the limit it saw more yellowing, higher haze, more gels and specks, and frequent bubble breakage.
The current natural PE film guideline lists SiOx and AlOx without additional coatings, plus EVOH up to 5 percent with PE-g-MAH tie layers, among the compatible barriers. In the extracted text it places metallisation and AlOx with a PVOH primer in a weaker column. The coloured PE film guideline lists metallisation alongside uncoated SiOx and AlOx. Those tables are hard to read in extract, so check the current text before you rely on the column placement. The RecyClass tool changelog shows PE flexible criteria were updated in March 2026.
Adhesives and inks count too. The same sheets set weight thresholds for polyurethane and acrylic adhesives and ask for testing when an adhesive is combined with a barrier other than EVOH or metallisation. For inks, the natural PE sheet points to a bleed test for retentive inks and says packaging printed on more than 30 percent of its surface needs a separate assessment.
Best for, by use
- Transparent pouch, dry oxygen-sensitive food in PE: PE/EVOH/PE with EVOH at or below 5 percent of weight, behind a BOPE or MDO-PE web. CloudFilm suggests snacks, confectionery, premium coffee and pet food often suit a BOPE outer with MDO-PE or PE inside.
- Transparent, humid fill or retort-adjacent: AlOx on a suitable base, with the flex caveat above. Jijid says retort-grade AlOx can reach OTR and WVTR of 2 or below.
- Light-sensitive, moisture-sensitive snack: metallised BOPP or BOPE. Confirm which PE guideline sheet your target market applies to metallisation.
- Stiffness and print without a high oxygen barrier (dry goods): BOPE/PE or MDO-PE/PE for PE streams, BOPP/CPP for PP; CloudFilm lists all three as options depending on local recycling guidance.
What this means for you
Ask suppliers for OTR and WVTR on the finished laminate, at the humidity you ship in, and after a flex or forming test. Request the EVOH weight as a percentage of the whole pouch, since 5 percent is the line RecyClass draws.
Run a first stack through the free tool: Free tool: laminate estimator gives indicative barrier and weight for a layer stack before you ask for samples. For typical resin and film values, Free tool: material properties table is a quick reference.
Resolve the recyclability question against the specific RecyClass sheet for your stream and market, then against the supplier data sheet. Grades vary; the data sheet decides. For quotes, ask your supplier.
Sources
- NOVA Chemicals: Oriented Polyethylene Films
- USPTO: Laminate structures and flexible packaging materials incorporating same (US 12059875)
- Dow via Entec: Biaxially Oriented Polyethylene TF-BOPE Resin
- Dow: Biaxially Oriented Polyethylene (BOPE) Films conference deck
- ScienceDirect Topics: Biaxially Oriented Polypropylene
- Aakash Poly Films: Transparent Non Heat Sealable BOPP Film
- Inteplast: BOPE Nonsealable Films
- Aropack: How to Specify Barrier Performance for Flexible Food Packaging
- Jijid: High Barrier Packaging Film Selection Guide
- BOBST: EVOH-free, Topcoat-free Transparent Solution for Full PE Barrier
- CloudFilm: Metallized BOPP Film
- CloudFilm: MDO PE vs BOPE
- CloudFilm: BOPP Vs BOPET Vs CPP Vs PE Packaging Film Guide
- Polifilm: Barrier Films
- Jindal Films: PP Mono-Material Solutions
- USPTO: High-barrier, metal oxide films (US 10718046)
- RecyClass: PE flexible films recycling, new findings for functional barriers
- RecyClass: Natural PE Flexible Films design for recycling guideline
- RecyClass: Coloured PE Flexible Films design for recycling guideline
- RecyClass tool: Guidelines
- PPWR EU: packaging regulation detail
Values are typical figures from the cited sources. Grades differ between suppliers. Check the supplier's data sheet and test your own structure before you decide.