BOPP, BOPE, MDO-PE, CPP and tie layers: a film glossary

Quick answer: this glossary is for packaging engineers, buyers, brand and quality colleagues who need to read a film spec or a laminate structure without a converter in the room. Read it top to bottom (process, named films, then layer joining), and use the table in the middle as a cheat sheet. In structures below, “//” marks a laminated join and “/” a coextruded layer boundary; suppliers vary, so ask.

This piece rests mainly on supplier pages (the film makers CloudFilm and VLM Poliplast, the converter National Flexible, and the packaging distributor Packaging Warehouse) and on patent documents. Independent test data is noted where it exists, which is rarely. Figures are typical values as checked on 15 November 2026, not specifications.

Making the film: five process terms

1. Orientation

Stretching a film while it is warm so the polymer chains line up in the direction of the pull. CloudFilm says this raises stiffness and dimensional stability, and its other pages add tensile strength and clarity. There is no single unit; the effect shows up as tensile modulus and strength (ASTM D882 is the usual film tensile method, and one patent cites ISO 527-3). It matters at the quote stage: an oriented film can be thinner than an unoriented one for the same job.

2. Machine direction (MD) and transverse direction (TD)

MD is the direction the web travels; TD is across it. Strength, elongation and shrink are quoted as MD/TD pairs. One distributor, Raghav Polymers, lists an 18 µm heat-sealable BOPP grade at 1,250 / 2,700 kg/cm2 tensile strength (about 123 / 265 MPa, our conversion), while Suprapol lists 200 / 160 MPa for a different grade. Two pages, two opposite balances: always read the data sheet for your grade and its test method.

3. Blown film

Polyethylene melt is extruded through a ring die and inflated into a bubble, then collapsed and wound. National Flexible’s explainer notes the bubble is blown vertically. It is a common route for PE film, and the starting point for MDO-PE below.

4. Cast film

Melt is pushed through a narrow flat slit, pulled away and cooled before winding, as one patent describes the process. Cast film is usually clearer and more uniform in thickness than blown film, though that general point comes from common practice rather than the sources used here. CPP is made this way.

5. Coextrusion

Two or more polymers are melted in separate extruders and joined in one die, so a multilayer film leaves the line in a single pass. Firsta Group describes a typical BOPP film as at least three layers, 15 to 60 µm in total, with a thick centre layer for mechanics and thinner outer layers for other duties. Layers are specified in µm each. Spec sheets show it as “A/B/C” structures.

The named films: BOPP, CPP, MDO-PE and BOPE

6. BOPP (biaxially oriented polypropylene)

Polypropylene stretched in both MD and TD. CBRHK gives a typical range of 12 to 40 µm and a density of about 0.90 g/cm3, with most food packaging in 18 to 25 µm. Suprapol’s table stops at 30 µm. It shows up as the clear, glossy or matte outer web of a snack pouch, and as label film.

Our calculation: CBRHK says a 20 µm BOPP can stand in where 30 to 40 µm of cast PP would be needed. Grammage is thickness times density: 20 µm × 0.90 g/cm3 = 18 g/m2, against 30 × 0.90 = 27 g/m2 and 40 × 0.90 = 36 g/m2. That is 9 to 18 g/m2 less, or 33 to 50 percent, if the claim holds for your pack. Free tool: the unit converter turns microns and density into gsm.

7. CPP (cast polypropylene)

Unoriented PP made on a cast line. CloudFilm calls it a soft film that works as the inner sealing or retort layer, in contrast to BOPP as the outer layer. Suprapol lists 15 to 50 µm, and a research paper describes a three-layer coextruded CPP seal film at 25 µm. Its job in the laminate is the inside face that meets the product.

8. MDO-PE (machine direction oriented polyethylene)

PE film stretched in the machine direction only, by rollers after the blown bubble stage (National Flexible). It is typically made at converters on blown lines. It is used as a stiff print web, often to replace a PET outer layer in an all-PE structure. The trade-off, per VLM, is that tear resistance drops along the direction of the draw.

9. BOPE (biaxially oriented polyethylene)

PE stretched in MD and TD on a stenter line like BOPP, which National Flexible says means it is made at BOPP film manufacturers. VLM says BOPE gives up some peak MD figure for properties closer to equal in both directions. CloudFilm suggests combining it with MDO-PE or PE-EVOH-PE films.

Film Stretched in Usual role Typical thickness (µm)
BOPP MD and TD Outer print web, label film 12 to 40 (CBRHK, CloudFilm); 12 to 30 (Suprapol)
CPP Not stretched (cast) Inner sealing layer 15 to 50 (Suprapol)
MDO-PE MD only Stiff print web in mono-PE Grade-dependent; ask supplier
BOPE MD and TD Print web replacing PET or PA Grade-dependent; ask supplier

Structures: mono-material laminates and tie layers

10. Mono-material laminate

A laminate where one polymer family makes up nearly all the pack, so it can go to one recycling stream. VLM’s working definition is at least 90 percent of a single polymer by mass. Examples from CloudFilm are BOPE // PE, or MDO-PE // PE-EVOH-PE // PE. Whether the pack is actually recycled depends on local collection; CloudFilm itself says this. For the EU rules on recyclability, which are changing, see ppwreu.org and check the current text.

11. Tie layer

A thin adhesive resin inside a coextruded film that bonds two polymers which would not otherwise stick, such as PE to EVOH or polyamide. A patent notes that maleic anhydride grafted polyolefins have been widely used for this in coextrusion and extrusion coating. Westlake’s TYMAX GT1057 data sheet is one example, a maleic anhydride modified LDPE for coextruded tie layers and laminating, adhering to polyolefins, polyamides, aluminium foil and EVOH.

A typical stack reads PE/tie/EVOH/tie/PE; another patent lists the PE/tie/EVOH/tie/PET variant. A different patent says maleic anhydride can react with EVOH and cause clarity problems, so acid terpolymers are an alternative. Delamination between layers is where this term turns up in complaints.

Joining and preparing: lamination and corona treatment

12. Lamination

Bonding two or more webs into one structure. A patent background names two classes: extrusion lamination and adhesive lamination. Packaging Warehouse adds thermal lamination, where a thermoplastic layer is activated and no curing is needed. Most adhesives are polyurethane-based, according to another patent. Ask which route your supplier uses, because it sets lead time.

13. Solvent-based lamination

Liquid adhesive is coated on one web and the solvent is dried off in a tunnel, which needs extraction for the fumes. Packaging Warehouse puts the curing time before further processing at roughly 12 to 24 hours. It is a common route for printed laminates with metallised film.

14. Solventless lamination

A two-component adhesive, usually polyurethane, is applied at close to 100 percent solids, so no drying tunnel is needed. Packaging Warehouse gives a cure time of 3 to 7 days; a patent background gives 2 to 5 days for two-component systems generally. The same patent notes heated application equipment and residual aromatic amines from isocyanate chemistry as limits, a point to raise with your food-contact compliance team. Cure time sits between printing and slitting, so it shows up as lead time.

Line speeds quoted for the methods are in the chart: the adhesive developer behind the second patent claims 100 to 200 m/min for solvent or water-based and 200 to 400 m/min for solventless; Packaging Warehouse gives 80 to 120 m/min for thermal lamination.

Quoted line speed ranges by lamination method. Low end of range: Thermal lamination 80, Solvent or water-based adhesive 100, Solventless adhesive 200; High end of range: Thermal lamination 120, Solvent or water-based adhesive 200, Solventless adhesive 400 (m/min)
Quoted line speed ranges by lamination method
Source: Packaging Warehouse (thermal); US 12252636 patent background (solvent/water-based and solventless), company claims

15. Corona treatment

An electrical discharge that raises the surface energy of PE or PP film so inks and adhesives wet and bond. The level is quoted in dyne/cm (1 dyne/cm equals 1 mN/m) and measured to ASTM D2578 (ISO 8296 is the ISO equivalent). With dyne solutions, the Enercon description is that the film’s level is the last solution that stays wetted for 2 seconds.

Sources disagree on the floor: Droplet Lab cites 35 dyne/cm as generally acceptable for flexo on PE, and a patent says 37 or higher depending on the adhesive. Treatment decays in storage, and another patent describes a target of above 35 dyne/cm after at least 7 days.

What this means for you

Some questions that follow from the entries above:

  • Name the direction. Ask for MD and TD values with the test method, not one tensile figure.
  • Ask for the layer map. Request the structure with each coextruded layer in µm, including which tie resin sits between which layers.
  • Say which orientation you mean. MDO-PE and BOPE are different films from different kinds of supplier, so a quote for one is not a quote for the other.
  • Ask for cure time and dyne at use. Get the lamination route, the cure time before slitting, and the dyne level at the time of printing or laminating, not only at the film line.
  • Treat “recyclable” as a claim to check before putting it on a pack.

To see how a stack of layers adds up in weight, try the laminate estimator (free tool: indicative layer stack weight from your own thicknesses).

Sources

Definitions follow the cited standards and sources. Terms can differ between regions and suppliers.

Header image: illustration, AI-generated.